Shear strength of concrete members
A concrete beam carries shear through the grip across its diagonal cracks and through the stirrups those cracks cross. How much of each it gets depends on how much the section is stretched, so the shear strength depends on the load, the moment and the prestress.
Sheet 2 · Longitudinal steel at the bearing
Shear also pulls on the bottom steel. Near a simple support the moment is small, but the strands are not yet fully gripped. Take Vs and θ from Sheet 1.
Key points
- Two shares. The concrete carries Vc, set by β (how well the crack faces grip). The stirrups carry Vs, set by how many of them the crack crosses: dv cot θ / s.
- The strain decides β and θ. More moment stretches the bottom steel, the cracks open, β falls and θ gets steeper. So the shear strength depends on the load, and a section away from the support can be critical.
- Prestress helps. It holds the strain at or below zero, which gives the best values: β = 4.8 and θ = 29° in the General Procedure.
- Three ways to get β and θ. The simplified method (β = 2, θ = 45°) suits reinforced sections with at least minimum stirrups. The General Procedure equations and the Appendix B5 tables both follow the strain; the tables give flatter cracks.
- Light stirrups cost twice. Below the minimum, the stirrups add little and β is cut for wider crack spacing. Adding stirrups up to the minimum raises Vc as well as Vs.
- Check the bottom steel near the bearing. The crack's diagonal push needs tension in the strands, where they are still building up their stress.
VDOT's BrR settings for LRFR rating use the General Procedure (not Appendix B5) for reinforced and prestressed concrete, take a negative strain as zero, and do not iterate. Design and legal load shear is not rated for members without shear distress (as MBE 6A.5.8 allows), but permit load shear is. The longitudinal steel check is ignored in rating. IIM-S&B-80.10 does not change the shear articles. VDOT-LR-G6 pp.25, 27; IIM-S&B-80.10
Quick check
On Sheet 1, Example 1, raise the moment Mu from 791 to 3,000 k-ft. φVn…
The moment now beats the prestress: the strain goes to about +1.4 × 10−3, β drops to 2.3 and θ rises to 34°. φVn falls from about 249 to 172 k, below Vu = 205 k. That is the moment–shear interaction.
Example 3 fails. Halve the stirrup spacing from 18 to 9 in. What happens to the concrete share Vc?
At 9 in. the stirrups meet the minimum, so β is no longer cut for crack spacing: Vc rises from about 70 to 83 k while Vs doubles. φVn goes from 82 to 113 k and passes.
On Sheet 2, Example 1, move the bearing edge from 9 in. to 3 in. from the girder end. The ratio…
The crack now meets the strands 12 in. from the end instead of 18 in., where they carry only about 65 ksi. The capacity falls from 418 to 279 k against the same 261 k demand: ratio 1.07.
Sources
- FHWA-NHI 130092, LRFR participant workbook, Lesson 14 (pp. 471–508); walk-through PW 14.18–14.34.
- AASHTO LRFD BDS 8th Ed.: 5.5.4.2 (resistance factors), 5.7.2.5 (minimum stirrups), 5.7.2.8 (shear stress, bv, dv), 5.7.3.2 (critical section), 5.7.3.3 (Vn, Vc, Vs), 5.7.3.4.1 and 5.7.3.4.2 (simplified and General Procedure), 5.7.3.5 (longitudinal reinforcement), 5.9.4.3 (transfer and development length), Appendix B5 and Table B5.2-1.
- AASHTO MBE 3rd Ed.: 6A.5.8 (shear rating of in-service concrete bridges).
- VDOT load rating guideline LR-G6, pp.25, 27 (BrR settings); IIM-S&B-80.10, pp.6–8.
- FHWA-HIF-22-025, Concrete Bridge Shear Load Rating Guide and Examples; FHWA-HIF-18-061 (shear rating and the load that gives RF = 1).
A study aid, not a substitute for the AASHTO LRFD, the MBE or an agency's rating procedures. Example numbers are illustrative.